List the different sizing faults &state the causes of these faults



List the different sizing faults &state the causes of these faults:


1. Size spot: Size mtl should be added gradually to the mixing tank for good mixing.If itis added at once, spot are appeared on the yarn.

2. Repeating warp streaks: This defect is due touneven tension in the pre-beam.

3. Shinnery: This defect due to the friction between the yarn & drying cylinder.

4. Sandy warp: Due to not crushed or grind the size mtl properly.

5. Ridge Beam: This fault occurs due to uneven distribution of yarn in wraith.

6. Hard sizing: If the size mtls are applied too much, the size becomes hard which causes hard sizing.

7. Improper drying:
Under drying > Bacteria form >  yarn breakage.Over drying > Hard sizing.

8. Sizing dropping: This defect due to not optimum the viscosity of the size solution.

9. Size stitching: Due toimproper drying after sizing.

10. Uneven sizing:
Due to over or under sizing.